Product No:HY-916
Brand:HONG YE SILICONE
Product Usage:HY-916 is soft printing silicone rubber developed for porcelain products ceramic tableware printing specially with excellent resilience & elasticity the liquid silicone very delicate without any impurities or particles. HONG YE JIE 's pad printing silicone rubber is developed for porcelain products, ceramic tableware printing specially, with excellent resilience & elasticity, the liquid silicone very delicate without any impurities or particles.

INTRODUCTION  
        Pad printing silicone of HONG YE JIE is two-component silicone, includes tin curing silicone type and platinum cure silicone type, flowable, vulcanizes at room temperature.
Can be used for a long time in the temperature range of - 65 ° C - 200 ° C and keep its soft and elastic properties.


APPLICATION

        HONG YE JIE 's pad printing silicone rubber is developed for porcelain products, ceramic tableware printing specially, with excellent resilience & elasticity, the liquid silicone very delicate without any impurities or particles.
HONG YE SILICONE is suitable for making printing pads, tampo pads for transfer patterns and contents to the porcelain /ceramics, plastic, electroplated products, toys, tableware and so on.


ADVANTAGES
* The liquid silicone very delicate without any impurities or particles.
* Excellent resilience & elasticity
* Durable, the printing times can more than 50000 times without sign of tearing or wearing on pads for some items.
* Good oil absorption effect
* The pattern is printed with great clarity and completeness.
* Keep good quality even though 200%-300% silicone oil added
* Low shrinkage
* No bubbles
* Adjustable with excellent antistatic performance


OPERATION INSTRUCTION
1.Mix part A and pars B evenly with correcte mixing ratio.
Notes: 1) Weigh the two parts exactly by electronic weight. For example, the operation time will be shorten after adding too much catalyst.
2)Mix part A and part B evenly. Otherwise the silicon rubber will be partly solidified which will make the finished molds meet a short life and waste silicon rubber.

2.Vacuum pumping
        Notes: 1) This step is not have to have, but it is best if there is one. It will discharge all air in the mixture  successfully, so as to ensure that there will be no bubbles in the finished silicone pad.
2) This step is less than 10 minutes. Otherwise, it
Will cause cross-linking reaction, and no more
further steps will be available.

3.Pouring
        We suggest to set the silicone pad for another 12 hours after demould before printing.